Questions concerning iron and steel, steel making, rod rolling, galvanizing, springs, nails, fencing, and patenting go here.

TOPIC: Drawing advice

Drawing advice 2 years 8 months ago #821

This question is posted on behalf of a reader; advice welcome:

Our online pickling and phosphating has gone out of order and the take-up stand gears have broken. I am unable to pickle and phosphate 7 mm and 8 mm high carbon wire rod and cannot draw it to 3 and 4 mm respectively, on my 8 block wire drawing machines. Could you please suggest any method (other than conventional pickling) - mechanical or chemical - so that I am able to draw the wire rods?
The administrator has disabled public write access.

Re: Drawing advice 2 years 8 months ago #822

With the information it seems it would be easier to repair or replace the broken gears than to get involved in other descaling processes. Options as follows:

1.-Chemical descaling in batch.
a) Acid tank protected for Hydrochloric or Sulphuric acid.
b) Rinse tanks.
c) Phosphate and Borax or equivalent solution tank.
d) Overhead or other type of crane.

2.- Mechanical (Mechanical Descalers from Manufacturers)
a)Pulleys to break the rod scale
b)Brushes, or types of grinding wheels,
c)Tank to add phosphate and Borax or equivalent.

Please give more information

Eduardo Anaya
Senior Consultant
INDEPA S.C.
Mexico City
Tel(011-52)555-407-7451
This email address is being protected from spambots. You need JavaScript enabled to view it.
The administrator has disabled public write access.

Re: Drawing advice 2 years 8 months ago #823

Thank you for the feedback; more information may be forthcoming directly from the reader.
The administrator has disabled public write access.