Waviness in the wire that is created by a surface defect that can stem from vibrations caused by too long a distance between the capstan and die, hard wire, too many/too few number of capstan wraps, improper die entry, stick slip conditions or too short/no die bearing. It can also be caused by low lubricant concentration or poor lubrication with an old coolant mixture.