Dead Zone Formation

A condition that occurs to metals inside a drawing die. This problem can be created when the material is drawn with too high of a cone angle, causing the metal to deform too much on the surface of the wire and not enough in the lower layers, creating a dead metal zone. The dead metal no longer takes part in the flow but is sheared off to form a chevron-shaped void that can result in a “cup and cone” type fracture.